Grade SUS 836L
Other Names
Corresponding Standard JIS G 4305-2021
Cold-rolled stainless steel plate, sheet and strip
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS 836L Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 19 24 5 -
Maximum Value 0.03 1 2 0.045 0.03 24 26 7 0.25
①Where necessary, –CP may be attached after the above symbol of grade to indicate that the product is a plate. Example SUS 310L-CP
②Where necessary, –CS may be attached after the above symbol of grade to indicate that the product is a strip. Example SUS304-CS
SUS 836L Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Solid Solution ≥640 ≥275 ≥40 ≤217
Approximate Comparison Table
Japan United States International Organization for Standardization European Standard
JIS UNS ISO Numerical Grade Numerical Grade
SUS836L N08367 X2NiCrMoN25-21-7 4478-083-67-U (1.4478)