Grade SUS 410L
Other Names
Corresponding Standard JIS G 4305-2021
Cold-rolled stainless steel plate, sheet and strip
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
Density 7.75 g/cm3
SUS 410L Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 11 -
Maximum Value 0.03 1 1 0.04 0.03 13.5 0.6
①Where necessary, –CP may be attached after the above symbol of grade to indicate that the product is a plate. Example SUS 310L-CP
②Where necessary, –CS may be attached after the above symbol of grade to indicate that the product is a strip. Example SUS304-CS
SUS 410L Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Annealing ≥360 ≥195 ≥22 ≤183
1 Approximate Comparison Table
China Taiwan, China Japan South Korea France
GB ISC CNS JIS KS NF EN/NF
022Cr12
(00Cr12)
S11203 401L SUS 410L STS 410L Z3CT 12
2 Approximate Comparison Table
China Japan South Korea
GB ISC JIS KS
022Cr12
(00Cr12)
S11203 SUS 410L STR 410L
3 Approximate Comparison Table
China Japan International Organization for Standardization European Standard
GB ISC JIS ISO Numerical Grade Numerical Grade
022Cr12
(00Cr12)
GB/T 20878-2024
S11203 SUS410L X2Cr12
ISO 15510
4030-410-90-X (1.4030)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!