Grade SUS 447J1
Other Names
Corresponding Standard JIS G 4305-2021
Cold-Rolled Stainless Steel Plate, Sheet and Strip
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
SUS 447J1 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N More
Minimum Value - - - - - 28.5 - - 1.5 - (Ni+Cu)≤0.50
Maximum Value 0.01 0.4 0.4 0.03 0.02 32 0.5 0.2 2.5 0.015
①Where necessary, –CP may be attached after the above symbol of grade to indicate that the product is a plate. Example SUS 310L-CP
②Where necessary, –CS may be attached after the above symbol of grade to indicate that the product is a strip. Example SUS304-CS
SUS 447J1 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Annealing ≥450 ≥295 ≥22 ≤207
1 Approximate Comparison Table Ferritic Stainless Steel
China Taiwan, China Japan South Korea
GB ISC CNS JIS KS
008Cr30Mo2
(00Cr30Mo2)
S13091 447J1 SUS 447J1 STS 447J1
2 Approximate Comparison Table Ferritic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S13091 SUS447J1 S44700 X1CrMo30-2 4135-447-92-C (1.4135)
SUS447J1 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!