Grade 20Cr
Corresponding Standard JB /T 6396-2006
Specification for The Heavy Alloy Structural Steel Forings
Classification Alloy Steel
20Cr Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.18 0.17 0.5 - - 0.7 -
Maximum Value 0.24 0.37 0.8 0.035 0.035 1 0.2
20Cr Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
15 (sample) Single quenching + tempering ≥835 ≥540 ≥10 ≥40 ≥250 ≥47
30 (sample) Double Quenching and Tempering ≥635 ≥390 ≥12 ≥40 ≥190 ≥47
≤60 Carburizing + Quenching + Tempering ≥635 ≥390 ≥13 ≥40 ≥190 ≥39

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!