Grade 16CrMn
Corresponding Standard JB /T 6396-2006
Specification for The Heavy Alloy Structural Steel Forings
Classification Alloy Steel
16CrMn Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value 0.14 0.17 1 - - 1 - -
Maximum Value 0.19 0.37 1.3 0.035 0.035 1.1 0.3 0.2
16CrMn Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
≤30 Carburizing + Quenching + Tempering 780~1080 ≥590 ≥10 ≥40 235~320 ≥34
31~63 Carburizing + Quenching + Tempering 640~930 ≥440 ≥11 ≥40 190~280 ≥34
16CrMn Corresponding Standards(Same grade name, different standards)