Grade 17Cr2Ni2Mo
Corresponding Standard JB /T 6396-2006
Specification for the heavy alloy structural steel forings
Classification Alloy Steel
17Cr2Ni2Mo Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.14 0.17 0.3 - - 1.5 1.4 - 0.25
Maximum Value 0.19 0.37 0.6 0.035 0.035 1.8 1.7 0.2 0.35
17Cr2Ni2Mo Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
ksi
Yield Point
σs
ksi
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
≤30 Carburizing + Quenching + Tempering 1080~1320 ≥790 ≥8 ≥35 320~390
31~63 Carburizing + Quenching + Tempering 980~1270 ≥690 ≥8 ≥35 290~375
17Cr2Ni2Mo Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!