Grade 18Cr2Ni4W
Corresponding Standard JB /T 6396-2006
Specification for the heavy alloy structural steel forings
Classification Alloy Steel
18Cr2Ni4W Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu W
Minimum Value 0.13 0.17 0.3 - - 1.35 4 - 0.8
Maximum Value 0.19 0.37 0.6 0.035 0.035 1.65 4.5 0.2 1.2
18Cr2Ni4W Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
≤80 Quenching + Tempering ≥1180 ≥835 ≥10 ≥45 ≥350 ≥78
81~100 Quenching + Tempering ≥1180 ≥835 ≥9 ≥40 ≥350 ≥74
101~150 Quenching + Tempering ≥1180 ≥835 ≥8 ≥35 ≥350 ≥70
151~250 Quenching + Tempering ≥1180 ≥835 ≥7 ≥30 ≥350 ≥66
18Cr2Ni4W Corresponding Standards(Same grade name, different standards)