Grade NCF718
Other Names
Corresponding Standard JIS G 4902-1991
Corrosion-Resisting and Heat-resisting Superalloy Plates and Sheets
Classification Nickel and Nickel Alloys
Properties Corrosion Resistance
NCF718 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti B Al More
Minimum Value - - - - - 17 50 - 2.8 0.65 - 0.2 Fe:余量;Nb+Ta:4.75~5.5
Maximum Value 0.08 0.35 0.35 0.015 0.015 21 55 0.3 3.3 1.15 0.006 0.8
NCF718 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Plate; t≤25 Solution Heat Treatment + Aging (H) ≥1240 ≥1035 ≥12
Plate; 25<t≤60 Solution Heat Treatment + Aging (H) ≥1240 ≥1035 ≥10
NCF718 Corresponding Standards(Same grade name, different standards)