Grade NCF751
Other Names
Corresponding Standard JIS G 4902-1991
Corrosion-Resisting and Heat-resisting Superalloy Plates and Sheets
Classification Nickel and Nickel Alloys
Properties Corrosion Resistance
NCF751 Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Cu Ti Al More
Minimum Value 5 - - - - - 14 70 - 2 0.9 Nb+Ta:0.7~1.2
Maximum Value 9 0.1 0.5 1 0.03 0.015 17 - 0.5 2.6 1.5
NCF751 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Plate; t≤100 Solution (S) - - - ≤375
Plate; t≤100 Solution Heat Treatment + Aging (H) ≥960 ≥615 ≥8 -
NCF751 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!