Grade SUS316TKC
Corresponding Standard JIS G 3446-2017
Stainless Steel Tubes for Machine and Structural Purposes
Classification Austenitic Stainless Steel
Properties Strength Corrosion Resistance Low-Temperature Toughness Impact Toughness
Density 7.98 g/cm3
SUS316TKC Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 16 10 2
Maximum Value 0.08 1 2 0.045 0.03 18 14 3
SUS316TKC Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe ≥520 ≥205 ≥35
Steel pipes; 1<t≤2 ≥26
Steel pipe; 2<t≤3 ≥28
Steel pipe; 3<t≤4 ≥29
Steel pipe; 4<t≤5 ≥30
Steel pipe; 5<t≤6 ≥32
Steel pipe; 6<t≤7 ≥34
Steel pipes; 7<t≤8 ≥35

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!