Grade SUS 316L-W1
Other Names
Corresponding Standard JIS G 4309-2013
Stainless steel wires
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS 316L-W1 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 16 12 2
Maximum Value 0.03 1 2 0.045 0.03 18 15 3
Symbol of temper and classification:
W1-soft No.1;W2-soft No.2;W1/2H-1/2 hard
SUS 316L-W1 Mechanical Properties
diameter
d
mm
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
0.02≤d≤0.05 650~900 ≥10
0.05<d≤0.16 650~900 ≥20
0.16<d≤0.5 610~860 ≥20
0.5<d≤1.6 570~820 ≥30
1.6<d≤5 520~770 ≥30
5<d≤14 500~750 ≥30

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!