Grade SUS 305J1-W2
Other Names
Corresponding Standard JIS G 4309-2013
Stainless steel wires
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS 305J1-W2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 16.5 11
Maximum Value 0.08 1 2 0.045 0.03 19 13.5
Symbol of temper and classification:
W1-soft No.1;W2-soft No.2;W1/2H-1/2 hard
SUS 305J1-W2 Mechanical Properties
diameter
d
mm
Tensile Strength
σb
Mpa
0.8≤d≤1.6 780~1130
1.6<d≤5 740~1080
5<d≤14 740~1030

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!