Grade C75S
European Standard Steel Grade 1.1248
Corresponding Standard EN 10132-4-2002
Classification Spring Steel
C75S Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.7 0.15 0.6 - - - - -
Maximum Value 0.8 0.35 0.9 0.025 0.025 0.4 0.4 0.1
C75S Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
0.3≤t≤3 Annealing (+A) or Annealing and Flattening (+LC) ≤640 ≤510 ≥15 HV
≤200
0.3≤t≤3 Cold Rolled (+CR) ≤1170 ≤320
0.3≤t≤3 Tempering (+QT) 1200~1900 370~580
Approximate Comparison Table Spring Steel
United States Germany France European Standard Russia Sweden United Kingdom
AISI UNS DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS14 BS EN/BS
1078 G10780 Ck75 1.1248 C75RR C75S 1.1248 75A 1774 CS80