Grade SUS410-HR
Corresponding Standard JIS G 4312-2019
Heat-Resistant Steel Plate, Sheet and Strip
Classification Martensitic Stainless Steel
Properties Corrosion Resistance
Density 7.75 g/cm3
SUS410-HR Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 11.5 -
Maximum Value 0.15 1 1 0.04 0.03 13.5 0.6
SUS410-HR Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Plates, strips Annealing ≥440 ≥205 ≥20 ≤201