Grade SUS316L-WSA
Other Names
Corresponding Standard JIS G 4315-2013
Stainless steel wires for cold heading and cold forging
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS316L-WSA Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 16 12 2
Maximum Value 0.03 1 2 0.045 0.03 18 15 3
SUS316L-WSA Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Wire rod; 0.8≤d<2 Solid Solution After Drawing 560~710 ≥20 ≥70
Wire; 2≤d≤5.5 Solid Solution After Drawing 510~660 ≥30 ≥70