Grade PCrMoV
Corresponding Standard GJB 3783A-2015
Specification for steel bars and steel forgings for barrel of middle-small caliber quick firing arms
Classification Alloy Steel
PCrMoV Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V
Minimum Value 0.32 0.17 0.25 - - 1 - - 0.2 0.1
Maximum Value 0.42 0.37 0.5 0.03 0.03 1.3 0.5 0.2 0.3 0.25
PCrMoV Mechanical Properties
condition Mark
Heat Treatment or Condition
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Steel bars or forgings, transverse sample; t=25 Strength Grade P-540 Normalizing + Quenching + Tempering Specified Proportional Limit σp
540
≥35 ≥17
Steel bars or forgings, transverse sample; t=25 Strength Grade P-590 Normalizing + Quenching + Tempering Specified Proportional Limit σp
590
≥35 ≥17
Steel bars or forgings, transverse sample; t=25 Strength Grade P-635 Normalizing + Quenching + Tempering Specified Proportional Limit σp
635
≥30 ≥17
Steel bars or forgings, transverse sample; t=25 Strength Grade P-685 Normalizing + Quenching + Tempering Specified Proportional Limit σp
685
≥30 ≥17
PCrMoV Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!