Grade G-X5CrNi 13 4
Germany W-Nr. 1.4313
Corresponding Standard DIN 17445-1984
Stainless Steel Castings -technical Delivery Conditions
Classification Cast Steel
Properties Corrosion Resistance
Density 7.7 g/cm3
G-X5CrNi 13 4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 12 3.5 -
Maximum Value 0.07 1 1.5 0.035 0.025 13.5 5 0.7
G-X5CrNi 13 4 Mechanical Properties
condition Test Temperature Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Casting Room Temperature Quenching + tempering, stage 1 760~960 ≥550 ≥15 240~300 ≥50
Casting Room Temperature Quenching + tempering, stage 2 900~1100 ≥830 ≥12 280~350 ≥35
Casting Quenching + tempering, stage 1 ≥515
≥500
≥485
≥470
≥455
≥440
Casting Quenching + tempering, stage 2 ≥810
≥770
≥750
≥725
≥700
≥680
1 Approximate Comparison Table Other Stainless Steels
Germany France European Standard Sweden United Kingdom
DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
X5CrNi 13-4 1.4313 Z25CN 13-4 X3CrNiMo 13-4 1.4313 2385 425C11
2 Approximate Comparison Table Heat-Resistant Cast Steels and Alloys
Japan Germany France United Kingdom
JIS DIN EN/DIN W-Nr. NF EN/NF BS EN/BS
SCS5
SCS6
G-X5CrNi13 4 1.4313 Z4CND13.4-M 425C1

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!