Grade 30CND 8
Corresponding Standard NF A 35-557-1983
Iron And Steel — Heat Treatable Steels for Externally Threaded, High Performance Fasteners for Engineering Purposes.
Classification Alloy Steel
Properties Strength
30CND 8 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.26 0.1 0.3 - - 1.8 1.8 0.3
Maximum Value 0.33 0.4 0.6 0.03 0.025 2.2 2.2 0.5
30CND 8 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar, Coil; d=50 Oil Quenching - - - HR48 -
Bar, coil; d ≤ 50 Quenching and Tempering 1130~1330 ≥950 ≥10 - Charpy U Notch
≥50
Approximate Comparison Table Structural Alloy Steel
China Japan International Organization for Standardization Germany France European Standard Russia United Kingdom
GB JIS ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST BS EN/BS
30Cr2Ni2Mo SNCM431 31CrNiMo8 30CrNiMo8 30CND8 30CrNiMo8 1.6580 3KH3M3F 823M30
30CND8 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!