Grade 37CrS4
European Standard Steel Grade 1.7038
Corresponding Standard EN 10083-3-2006
Classification Alloy Steel
37CrS4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value 0.34 - 0.6 - 0.02 0.9
Maximum Value 0.41 0.4 0.9 0.025 0.04 1.2
• Elements not quoted in this table shall not be intentionally added to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat and for boron to have its effect on the hardenability. All reasonable precautions shall be taken to prevent the addition of such elements from scrap or other material used in the manufacture which affect the hardenability, mechanical properties and applicability.
Approximate Comparison Table Alloy Steel for Quenching and Tempering
International Organization for Standardization Germany France European Standard
ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
37CrS4 37CrS4 1.7038 38C4u 37CrS4 1.7038