Grade GH4043
Old Grade
Corresponding Standard GB /T 14993-1994
Hot-Rolled Heat-resisting Superalloy Bars for Rotating Parts
Classification Special Alloy Steel
GH4043 Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Cu Mo As Ti W Nb B Pb Al Sn Ce Bi Sb More
Minimum Value - - - - - - 15 - 4 - 1.9 2 0.5 - - 1 - - - - Ni余量
Maximum Value 5 0.12 0.6 0.5 0.015 0.01 19 0.07 6 0.0025 2.8 3.5 1.3 0.01 0.001 1.7 0.0012 0.03 0.001 0.0025
GH4043 Mechanical Properties
condition Test Temperature Mark
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Rod Room Temperature Indentation diameter (mm)
3.3~3.7
Rod High temperature instantaneous tensile properties ≥686 ≥6 ≥10
Rod High-Temperature Endurance Performance Stress 275MPa; Time ≥50h
Rod High-Temperature Endurance Performance Stress (245MPa); Time ≥ (100h)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!