Grade 41CrNiMo2E
Old Grade
Corresponding Standard JIS G 7401-2000
Steels for cold heading and cold extruding
Classification Alloy Steel
41CrNiMo2E Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.37 - 0.7 - - 0.4 0.4 0.15
Maximum Value 0.44 0.4 1 0.035 0.035 0.6 0.7 0.3
41CrNiMo2E Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Cold heading steel AC or AC+P ≤650 ≥55
Cold heading steel C+AC ≤630 ≥57
Cold heading steel C+AC+LC ≤660 ≥57
U-untreated with hot-rolled surface;P-untreated with peeled surface;C-cold drawn;AC-annealed to achive spheroidization of the carbides;AC+P-annealed to achive spheroidization of the carbides and peeled;C+AC-cold drawn and annealed to achive spheroidization of the carbides;C+AC+LC-cold drawn and annealed to achive spheroidization of the carbides, and lightly cold reduced (e.g. with a reduction of 5%)
41CrNiMo2E Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!