Grade 31CrNiMo8E
Old Grade
Corresponding Standard JIS G 7401-2000
Steels for cold heading and cold extruding
Classification Alloy Steel
31CrNiMo8E Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.27 - 0.3 - - 1.8 1.8 0.3
Maximum Value 0.34 0.4 0.6 0.035 0.035 2.2 2.2 0.5
31CrNiMo8E Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Cold heading steel AC or AC+P ≤700 ≥58
Cold heading steel C+AC ≤680 ≥60
Cold heading steel C+AC+LC ≤710 ≥60
U-untreated with hot-rolled surface;P-untreated with peeled surface;C-cold drawn;AC-annealed to achive spheroidization of the carbides;AC+P-annealed to achive spheroidization of the carbides and peeled;C+AC-cold drawn and annealed to achive spheroidization of the carbides;C+AC+LC-cold drawn and annealed to achive spheroidization of the carbides, and lightly cold reduced (e.g. with a reduction of 5%)