Grade 6101
Other Names
Corresponding Standard JIS H 4040-2015
Aluminium and Aluminium Alloy Bars and Wires
Classification Aluminum and Aluminum Alloys
6101 Chemical Element Composition Content (%)
Component Fe Si Mn Cr Cu B Zn Mg More
Minimum Value - 0.3 - - - - - 0.35 Al:余量
Maximum Value 0.5 0.7 0.03 0.03 0.1 0.06 0.1 0.8
6101 Mechanical Properties
condition Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Extruded bar (BE); 3≤d≤7 A6101 T6 Solid Solution Heat Treatment + Artificial Aging (T6) ≥195 ≥165 A50mm
≥10
Extruded Bar (BE); 7<d≤17 Solid Solution Heat Treatment + Artificial Aging (T6) ≥195 ≥165 ≥12
Extruded Bar (BE); 17<d≤30 Solid Solution Heat Treatment + Artificial Aging (T6) ≥175 ≥145 ≥14
Extruded bar (BE); 3≤d≤17 A6101 T7 Solution heat treatment + stabilization (T7) ≥135 ≥110 ≥10
① A50mm、A(5.65√S0)- gauge length,S0-Specimen area,s=S0,unit mm sq
② d-diameter、thickness or width across flats, unit mm;s - cross section area, unit mm sq
6101 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!