Grade C1751
Other Names
Corresponding Standard JIS H 3130-2018
Copper beryllium alloy, copper titanium alloy, phosphor brozne, copper-nickel-tin alloy and nickel silver sheets, plates and strips for springs
Classification Copper and Copper Alloys
Properties High Elasticity Corrosion Resistance
C1751 Chemical Element Composition Content (%)
Component Be Ni More
Minimum Value 0.2 1.4 Cu+Be+Ni≥99.5
Maximum Value 0.6 2.2
C1751 Mechanical Properties
condition Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Plate (P), strip (R); 0.10≤t≤0.6 C1751 P-OM,C1751 R-OM OM 690~895 ≥550 ≥10 HV
≥210
Plate (P), strip (R); 0.10≤t≤0.6 C1751 P-HM,C1751 R-HM HM 760~965 ≥655 ≥5 ≥230
Approximate Comparison Table Processing of High Copper Alloys
China Japan United States International Organization for Standardization Germany European Standard Russia
GB ISC JIS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. EN Numerical Grade GOST
TBe0.4-1.8
QBe0.4-1.8
C17510 C1751
C17510
97.8Cu-.4Be-1.8Ni C17510 CuNi2Be0.4 C17510 CuNi2Be C17510
2.0850
CuNi2Be CW110C БрБН0.4-1.8

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!