Grade Wieland-K88
Classification Copper and Copper Alloys
Wieland-K88 Chemical Element Composition Content (%)
Component C Si Cr Ti Ag More
Nominal Value 0.08 0.03 0.5 0.06 0.2 Cu:余量
Wieland-K88 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Rolled products R480 480~560 ≥450 L0=50
≥7
HV (For Reference Only)
140~170
Rolled products R540 540~630 ≥520 L0=50
≥2
HV (For Reference Only)
150~180
Rolled products TR08 520~620 ≥500 L0=50
≥7
HV (For Reference Only)
160~190

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!