Grade 20CrNi3
China ISC A42202
Corresponding Standard GB /T 3077-2015
Alloy structure steels
Classification Alloy Steel
Properties Strength Low-Temperature Toughness Carburizing Ability
Density 7.88 g/cm3
20CrNi3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.17 0.17 0.3 - - 0.6 2.75 - -
Maximum Value 0.24 0.37 0.6 0.03 0.03 0.9 3.15 0.3 0.1
20CrNi3 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=25 Quenching + Tempering ≥930 ≥735 ≥11 ≥55 ≤241 ≥78
Approximate Comparison Table Structural Alloy Steel
China France Russia
GB ISC NF EN/NF GOST
20CrNi3 A42202 20NC11 20ХН3А
20CrNi3 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!