Grade 35NiCr6
1.5815
Corresponding Standard NF EN 10083-3-2006
Steels for Quenching and Tempering - Part 3: Technical Delivery Conditions for Alloy Steels
Classification Alloy Steel
35NiCr6 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.3 - 0.6 - - 0.8 1.2
Maximum Value 0.37 0.4 0.9 0.025 0.025 1.1 1.6
35NiCr6 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Steel: d ≤ 16mm; t ≤ 8mm Quenching + Tempering (+QT) 880~1080 ≥740 ≥12 ≥40
Steel: 16mm ≤ d ≤ 40mm; 8mm ≤ t ≤ 20mm Quenching + Tempering (+QT) 880~1080 ≥740 ≥14 ≥40 ≥35
Steel: 40mm ≤ d ≤ 100mm; 20mm ≤ t ≤ 60mm Quenching + Tempering (+QT) 780~980 ≥640 ≥15 ≥40 ≥35
Steel: Processed to a Certain Shearability (+S)
Steel: Softening Annealing (+A) ≤223
35NiCr6 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!