Grade X7CrNiNb18-10
European Standard Steel Grade 1.4912
Corresponding Standard EN 10222-5-2017
Steel Forgings for Pressure Purposes - Part 5: Martensitic, Austenitic and Austenitic-Ferritic Stainless Steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X7CrNiNb18-10 Chemical Element Composition Content (%)
Component C Si Mn P S * Cr Ni More
Minimum Value 0.04 - - - - 17 9 Nb:10×C ~ 1.20
Maximum Value 0.1 1 2 0.045 0.015 19 12
X7CrNiNb18-10 Mechanical Properties
condition Test Temperature Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Cross-sectional thickness t≤450 +AT 510~710 ≥205 long. ≥40;tr. ≥30 long.≥100;tr.≥60
Cross-sectional thickness t≤450 +AT tr.≥40
Steel +AT ≥410 ≥171
Steel ≥390 ≥162
Steel ≥370 ≥153
Steel ≥360 ≥147
Steel ≥350 ≥139
Steel ≥345 ≥133
Steel ≥340 ≥129
Steel ≥330 ≥124
Steel ≥300 ≥121
1 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization France European Standard
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade NF EN/NF EN Numerical Grade
07Cr18Ni11Nb
(1Cr19Ni11Nb)
S34779 SUS347H 347H S34709 X7CrNiNb18-10 4912-347-09-I Z2CND17-11
Z2CND18-13
Z8CNNb18-10
X7CrNiNb18-10 1.4912
2 Approximate Comparison Table Seamless Steel Tubes and Pipes for High Pressure Boiler
China United States European Standard
GB ISC ASTM/AISI EN
07Cr18Ni11Nb S34779 SA-213 TP347H X7CrNiNb18-10

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!