Grade 317S16
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
317S16 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti Nb
Minimum Value - 0.2 0.5 - - 17.5 12 - 3 - -
Maximum Value 0.06 1 2 0.045 0.03 19.5 15 0.5 4 0.1 0.2
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States Germany United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3 S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States Germany United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3
(0Cr19Ni13Mo3)
S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
3 Approximate Comparison Table
China Japan United States International Organization for Standardization Russia United Kingdom
GB JIS ASTM/AISI ISO GOST BS EN/BS
0Cr19Ni13Mo3 SUS317 317 25 08X17H15M3T 317S16
317S16 Corresponding Standards(Same grade name, different standards)