Grade 30CrNiV9
Germany W-Nr. 1.7707
Corresponding Standard DIN 17204-1990
Seamless Circular Tubes Made from Steels for Quenching and Tempering Technical Delivery Conditions
Classification Alloy Steel
30CrNiV9 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo V
Minimum Value 0.26 - 0.4 - - 2.3 0.15 0.1
Maximum Value 0.34 0.4 0.7 0.035 0.035 2.7 0.25 0.2
30CrNiV9 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Hot drawn, cold drawn pipes Annealing ≤248
Pipes t≤8 Quenching + Tempering (V) 1250~1450 ≥1050 ≥9(long.);≥7tr.) ≥35
Pipes; 8< t≤20 Quenching + Tempering (V) 1250~1450 ≥1050 ≥9(long.);≥7(tr.) ≥35 *
≥25
Pipes; 20< t≤50 Quenching + Tempering (V) 1100~1300 ≥900 ≥10(long.);≥8(tr.) ≥40 ≥30
Pipe; 50<t≤80 Quenching + Tempering (V) 1000~1200 ≥800 ≥11(long.);≥9(tr.) ≥45 ≥35
Approximate Comparison Table Structural Alloy Steel
China Germany European Standard
GB DIN EN/DIN W-Nr. EN Numerical Grade
30Cr2MoV 30CrMoV9 1.7707 30CrMoV9 1.7707

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!