Grade CuNi12Zn24
Germany W-Nr. 2.0730
Corresponding Standard DIN 17671-1-1983
Wrought copper and copper alloys tube;Properties.
Classification Copper and Copper Alloys
Properties Corrosion Resistance
Density 8.7 g/cm3
CuNi12Zn24 Chemical Element Composition Content (%)
Component Fe Mn Ni Cu Pb Sn Other Total More
Minimum Value - - 11 63 - - - Zn:余量
Maximum Value 0.3 0.5 13 66 0.03 0.03 0.2
"Other individual elements or other totals": The chemical composition includes elements not specified in the table. Analysis should only be conducted if these elements are suspected to be present, or if routine analysis suggests that their content may exceed the prescribed limits.
CuNi12Zn24 Mechanical Properties
thickness
t
mm
Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Pipe; wall thickness as per agreement 2.0730.08 Extrusion or Hot Forging P (.08) No specification No specification No specification No specification
Pipes; t<3 2.0730.10 Soft F34 (.10) 340~420 ≤290 ≥45 ≈85
Pipes; t<3 2.0730.26 Half hard F42(.26) 420~490 ≥240 ≥28 ≈125
Pipes; t<2 2.0730.30 Hard F49(.30) ≥490 ≥390 ≥12 ≈150
Approximate Comparison Table Cupper and cupper alloy
Germany European Standard
DIN EN/DIN W-Nr. EN Numerical Grade
CuNi12Zn24 2.0730 CuNi12Zn24 CW403J

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!