Grade CuAl10Ni5Fe4
Germany W-Nr. 2.0966
Old Grade
Corresponding Standard DIN 17671-1-1983
Wrought copper and copper alloys tube;Properties.
Classification Copper and Copper Alloys
Properties Corrosion Resistance
Density 7.5 g/cm3
CuAl10Ni5Fe4 Chemical Element Composition Content (%)
Component Fe Mn Ni Pb Al ** Zn * Other Total More
Minimum Value 2 - 4 - 8.5 - - Cu:余量
Maximum Value 5 1.5 6 0.05 11 0.5 0.3
"Other individual elements or other totals": The chemical composition includes elements not specified in the table. Analysis should only be conducted if these elements are suspected to be present, or if routine analysis suggests that their content may exceed the prescribed limits.
CuAl10Ni5Fe4 Mechanical Properties
thickness
t
mm
Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Pipe; wall thickness as per agreement 2.0966.08 Extrusion or Hot Forging P (.08) No specification No specification No specification No specification
Pipes; 4≤t<12 2.0966.97 Semi-finished product + special treatment F64(.97) ≥640 ≥340 ≥10 ≈180
Approximate Comparison Table Cupper and cupper alloy
Japan United States International Organization for Standardization Germany France European Standard Russia United Kingdom
JIS UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST BS EN/BS
C6301 C63000 CuAl10Ni5Fe4 CuAl10Ni5Fe4 2.0966 CuAl9Ni5Fe3 CuAl10Ni5Fe4 CW307G BrAZHN10-4-4 CA104

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!