Grade X46Cr13
1.4034
Corresponding Standard NF EN 10088-2-2005
Part2:Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
Classification Martensitic Stainless Steel
X46Cr13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value 0.43 - - - - 12.5
Maximum Value 0.5 1 1 0.04 0.015 14.5
◎ Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. All appropriate precautions are to be taken to avoid the addition of such elements from scrap and other materials used in production which would impair mechanical properties and the suitability of the steel.
X46Cr13 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Cold rolled strip steel: T ≤ 8mm +A ≤780 ≥ 12① HRB:≤ 99 ; HB/HV:≤ 245
Hot rolled strip steel: T ≤ 13.5mm +A ≤780 ≥ 12① HRB:≤ 99 ; HB/HV:≤ 245
◎ T-thickness;l-longitudinal;t-trasverse
◎ +A=soft annealed;+QT=quenched and tempered;+P=precipitation hardened;+AT=solutiong annealed;+SR=strength relieved

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!