Grade X11CrNiMnN19-8-6
1.4369
Corresponding Standard NF EN 10088-2-2005
Part2:Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
Classification Austenitic Stainless Steel
X11CrNiMnN19-8-6 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value 0.07 0.5 5 - - 17.5 6.5 0.2
Maximum Value 0.15 1 7.5 0.03 0.015 19.5 8.5 0.3
◎ Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. All appropriate precautions are to be taken to avoid the addition of such elements from scrap and other materials used in production which would impair mechanical properties and the suitability of the steel.
X11CrNiMnN19-8-6 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Cold Rolled Steel Strip: T ≤ 4mm +AT 750~950 ( t )
Rp0.2:≥ 340①③
Rp1.0:≥ 370①②
( t )
T<3mm:≥35③④
T ≥ 3mm:≥35③⑤
Steel (Process Flow 2H): Cold working + C850⑥⑦ 850~1000
Steel (Process Flow 2H): Cold working + C1000⑥⑦ 1000~1150
Steel (Process Flow 2H): Cold work + C1150⑥⑦ 1150~1300
Steel (Process Flow 2H): Cold processing + C1300⑥⑦⑧ 1300~1500
Steel (Process Flow 2H): Cold working + CP500⑥⑦ 500~700
Steel (Process Flow 2H): Cold working + CP700⑥⑦ 700~900
Steel (Process Flow 2H): Cold work + CP900⑥⑦ 900~1100
Steel (Process Flow 2H): Cold work + CP1100⑥⑦ 1100~1300
◎ T-thickness;l-longitudinal;t-trasverse
◎ +A=soft annealed;+QT=quenched and tempered;+P=precipitation hardened;+AT=solutiong annealed;+SR=strength relieved