Grade 35SPb20
1.0756
Corresponding Standard NF EN 10087-1999
Free-cutting structural steels
Classification Carbon Steel
35SPb20 Chemical Element Composition Content (%)
Component C Si Mn P S Pb
Minimum Value 0.32 - 0.7 - 0.15 0.15
Maximum Value 0.39 0.4 1.1 0.06 0.25 0.35
35SPb20 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Steel: 5≤ d ≤10 Untreated State 550~720
Steel: 10<d ≤16 Untreated State 550~700
Steel: 16 < d ≤ 40 Untreated State 520~680 154~201
Steel: 40 < d ≤ 63 Untreated State 520~670 154~198
Steel: 63 < d ≤ 100 Untreated State 500~650 149~193
Steel: 5≤ d ≤10 Quenching + Tempering (+QT) 630~780 ≥430 ≥15
Steel: 10<d ≤16 Quenching + Tempering (+QT) 630~780 ≥430 ≥15
Steel: 16 < d ≤ 40 Quenching + Tempering (+QT) 600~750 ≥380 ≥16
Steel: 40 < d ≤ 63 Quenching + Tempering (+QT) 550~700 ≥320 ≥17
Steel: 63 < d ≤ 100 Quenching + Tempering (+QT) 550~700 ≥320 ≥17