Grade 44SMn28
1.0762
Corresponding Standard NF EN 10087-1999
Free-cutting structural steels
Classification Carbon Steel
44SMn28 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.4 - 1.3 - 0.24
Maximum Value 0.48 0.4 1.7 0.06 0.33
44SMn28 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Steel: 5≤ d ≤10 Untreated State 630~900
Steel: 10<d ≤16 Untreated State 630~850
Steel: 16 < d ≤ 40 Untreated State 630~820 178~242
Steel: 40 < d ≤ 63 Untreated State 620~790 184~235
Steel: 63 < d ≤ 100 Untreated State 610~780 181~231
Steel: 5≤ d ≤10 Quenching + Tempering (+QT) 700~850 ≥520 ≥16
Steel: 10<d ≤16 Quenching + Tempering (+QT) 700~850 ≥480 ≥16
Steel: 16 < d ≤ 40 Quenching + Tempering (+QT) 700~850 ≥420 ≥16
Steel: 40 < d ≤ 63 Quenching + Tempering (+QT) 700~850 ≥410 ≥16
Steel: 63 < d ≤ 100 Quenching + Tempering (+QT) 700~850 ≥400 ≥16

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!