Grade NiCr23Fe
Germany W-Nr. 2.4851
Corresponding Standard DIN 17752-2002
Wrought nickel and nickel alloy rod and bars Requirements and testing
Classification Nickel and Nickel Alloys
Properties Corrosion Resistance
Density 8.2 g/cm3
NiCr23Fe Chemical Element Composition Content (%)
Component Fe C * Si Mn P S Cr Ni Cu Ti B Co Al
Minimum Value - - - - - - 21 58 - - - - 1
Maximum Value 18 0.1 0.5 1 0.02 0.015 25 63 0.5 0.5 0.006 1.5 1.7
NiCr23Fe Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bar; d≤100 Solution heat treatment (F55) ≥550 ≥205 ≥30 ≤220 HBW2.5/62.5
Approximate Comparison Table corrosion-resistant alloy
China Japan South Korea United States Germany
GB ISC JIS KS Commercial Grade UNS W-Nr. L-Nr.
NS 3103
(NS 313)
(1Cr23Ni60Fe13Al)
H 06601
H 03103
NCF 601 NCF 601 Inconel 601 N 06601 NiCr23Fe 2.4851
NiCr23Fe Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!