Grade NiCr21Mo14W
Germany W-Nr. 2.4602
Corresponding Standard DIN 17752-2002
Wrought nickel and nickel alloy rod and bars Requirements and testing
Classification Nickel and Nickel Alloys
Properties Corrosion Resistance
Density 8.7 g/cm3
NiCr21Mo14W Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Mo W V Co More
Minimum Value 2 - - - - - 20 12.5 2.5 - - Ni:余量
Maximum Value 6 0.01 0.08 0.5 0.025 0.015 22.5 14.5 3.5 0.35 2.5
NiCr21Mo14W Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bars; d≤160 Solution Heat Treatment (F69) ≥690 ≥310 ≥45 ≤240 HBW2.5/62.5
1 Approximate Comparison Table corrosion-resistant alloy
China United States Germany
GB ISC Commercial Grade UNS DIN EN/DIN W-Nr.
NS 3308 H 06022
H 03308
Hastelloy C -22
Inconel 622
N 06022 NiCr21Mo14W
Nicrofer 5621 hMoW
2.4602
2 Approximate Comparison Table
United States Germany France United Kingdom
Commercial Grade AMS W-Nr. L-Nr. NF EN/NF BS EN/BS
Hastelloy C AMS5388D 2.4602 2.4537 ARC6015
NC17DWY
BSANC16
NiCr21Mo14W Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!