Grade NiCr22Mo7Cu
Germany W-Nr. 2.4619
Corresponding Standard DIN 17752-2002
Wrought nickel and nickel alloy rod and bars Requirements and testing
Classification Nickel and Nickel Alloys
Properties Corrosion Resistance
Density 8.3 g/cm3
NiCr22Mo7Cu Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Cu Mo W Co More
Minimum Value 18 - - - - - 21 1.5 6 - - Ni:余量;Na+Ta≤0.5
Maximum Value 21 0.015 1 1 0.025 0.015 23.5 2.5 8 1.5 5
NiCr22Mo7Cu Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bar; d≤20 Solution treatment (F62) ≥620 ≥240 ≥45 ≤240 HBW2.5/62.5
Bar; 20<d≤55 Solution heat treatment (F59) ≥590 ≥205 ≥35 ≤240 HBW2.5/62.5
Approximate Comparison Table Corrosion-Resistant Alloy
China United States Germany
GB ISC Commercial Grade UNS DIN EN/DIN W-Nr.
NS 3403
BG 2250
H 06985
H 03403
Hastelloy G-3 N 06985 Nicrofer 4023 hMo 2.4619
NiCr22Mo7Cu Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!