Grade NiCo20Cr20MoTi
Germany W-Nr. 2.4650
Corresponding Standard DIN 17752-2002
Wrought nickel and nickel alloy rod and bars Requirements and testing
Classification Nickel and Nickel Alloys
Properties Corrosion Resistance
Density 8.4 g/cm3
NiCo20Cr20MoTi Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Cu Mo Ti B Co Al More
Minimum Value - 0.04 - - - - 19 - 5.6 1.9 - 19 0.3 Ni:余量;Ti+Al:2.4~2.8
Maximum Value 0.7 0.08 0.4 0.6 0.02 0.015 21 0.2 6.1 2.4 0.005 21 0.6
NiCo20Cr20MoTi Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bars; d≤160 Solution treatment + aging treatment (F54) ≥540 ≥400 ≥12 ≈230 HBW2.5/62.5
Approximate Comparison Table Deformed High-Temperature Alloy
China Germany France United Kingdom
GB ISC DIN EN/DIN W-Nr. NF EN/NF BS EN/BS
GH4163
(GH163)
H41630 NiCo20Cr20MoTi 2.4650 ATG W0
NCK20D
HR10
HR 206
N263

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!