Grade NiCr22W14Mo
Germany W-Nr. 2.4733
Corresponding Standard DIN 17752-2002
Wrought nickel and nickel alloy rod and bars Requirements and testing
Classification Nickel and Nickel Alloys
Properties Corrosion Resistance
Density 9 g/cm3
NiCr22W14Mo Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Cu Mo Ti W B Co Al La More
Minimum Value - 0.05 0.25 0.3 - - 20 - 1 - 13 - - 0.2 0.005 Ni:余量
Maximum Value 3 0.15 0.75 1 0.02 0.015 24 0.5 3 0.1 15 0.015 5 0.5 0.05
NiCr22W14Mo Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Bar stock; d≤150 Solution treatment (F76)
≥760

≥310

≥35
NiCr22W14Mo Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!