Performance Level LF415K1
Corresponding Standard GB /T 14383-2021
Forged Fitting, Socket-Welding and Threaded
Classification Carbon Steel
LF415K1 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V
Minimum Value - 0.1 0.6 - - - - - - -
Maximum Value 0.3 0.4 1.05 0.025 0.02 0.3 0.4 0.4 0.12 0.08
LF415K1 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
≥415 ≥240 ≥22 ≥30 ≤160 -20°C;≥18
① Yield Point: For pipe fittings of the stainless steel category, the specified non-proportional elongation strength Rp0.2 is used. For pipe fittings of other material categories, when the lower yield strength ReL is not clearly defined, the specified non-proportional elongation strength Rp0.2 is used.