Performance Level LF485K2
Corresponding Standard GB /T 14383-2021
Forged Fitting, Socket-Welding and Threaded
Classification Carbon Steel
LF485K2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V Nb
Minimum Value - 0.15 0.6 - - - - - - - -
Maximum Value 0.3 0.6 1.6 0.025 0.02 0.3 0.4 0.4 0.12 0.08 0.03
LF485K2 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
485~655 ≥250 ≥20 ≥30 ≤197 -46°C;≥27
① Yield Point: For pipe fittings of the stainless steel category, the specified non-proportional elongation strength Rp0.2 is used. For pipe fittings of other material categories, when the lower yield strength ReL is not clearly defined, the specified non-proportional elongation strength Rp0.2 is used.

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!