Grade X1CrNiMoN25-22-2
1.4466
Corresponding Standard NF EN 10028-7-2008
Flat products made of steels for pressure purposes - Part 7 : stainless steels
Classification Austenitic Stainless Steel
X1CrNiMoN25-22-2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 24 21 2 0.1
Maximum Value 0.02 0.7 2 0.025 0.01 26 23 2.5 0.16
◎ Elements not quoted in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. All precautions are to be taken to avoid the addition of such elements from scrap and other materials used in production which would impair mechanical properties and the suitability of the steel.
X1CrNiMoN25-22-2 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
P:T ≤ 75 +AT 540~740 Rp0.2:≥250
Rp1.0:≥290
①②
T < 3mm: ≥40
T ≥ 3mm: ≥ 40
②③
20℃:
(l: ≥100;t: ≥60)
-196℃:
(t: ≥60)
◎ C-Cold rolled strip;H-Hot rolled strip;P-Hot rolled plate;T-Thickness;t-transverse;l-Longitudinal
◎ +A=annealed;+AT=solution annealed;+QT = quenched and tempered;+RA=recrystallizing annealed condition
Approximate Comparison Table
China United States International Organization for Standardization Germany France European Standard
GB ISC ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
022Cr25Ni22Mo2N S31053 310MoLN S31050 X1CrNiMoN 25-22-2 X1CrNiMoN 25-22-2 1.4466 X1CrNiMoN 25-22-2 X1CrNiMoN 25-22-2 1.4466