Grade 42CrMo
Corresponding Standard GB /T 18248-2021
Seamless steel tubes for gas cylinder
Classification Alloy Steel
42CrMo Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo More
Minimum Value 0.38 0.17 0.5 - - 0.9 - - 0.15 P+S≤0.025;V+Nb+Ti+B+Zr≤0.15ⓐ
Maximum Value 0.45 0.37 0.8 0.02 0.01 1.2 0.3 0.2 0.25
42CrMo Mechanical Properties
condition Test Temperature Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Steel pipe specimen Room Temperature 830~870°C Quenching (Normalizing), Oil Cooling + 510~610°C Tempering, Water, Oil Cooling ≥1080 ≥930 ≥12 ≥27(-50°C)
Steel pipe specimen Room Temperature Tempering ≥930 ≥760 ≥14②
Steel pipe outer diameter D>140mm; t=3*~5, Transverse Tempering ≥30③;≥24④
Steel pipe outer diameter D>140mm; t=5~7.5, Transverse Tempering ≥35③;≥28④
Steel pipe outer diameter D>140mm; t=7.5~10, Transverse Tempering ≥40③;≥32④
Steel pipe outer diameter D≤140mm; t=3~10, Longitudinal Tempering ≥60③;≥48④
1 Approximate Comparison Table Structural Alloy Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS14 BS EN/BS
42CrMo A30422 SCM440 SCM440
SCM440H
SCM440 4140
4142
G41400
G41420
42CrMo4 42CrMo4 1.7225 42CD4 42CrMo4 1.7225 2244 708M40
2 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
42CrMo SCM440H 4140
4142
42CrMo4 42CrMo4 42CD4 42CrMo4 1.7225 35KHM
38KHM
2244 708M40
CFS11
3 Approximate Comparison Table Structural Alloy Steel
China United States
GB ASTM
42CrMo A193 B7