Grade X1NiCrMoCu 31-27-4
European Standard Steel Grade 1.4563
Corresponding Standard EN 10250-4-1999
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X1NiCrMoCu 31-27-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 26 30 0.7 3 -
Maximum Value 0.02 0.7 2 0.03 0.01 28 32 1.5 4 0.11
X1NiCrMoCu 31-27-4 Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤250* 500~750 ≥220 ≥30 ≥100
t≤250** 500~750 ≥220 ≥30 ≥60
1 Approximate Comparison Table corrosion-resistant alloy
China United States Germany
GB ISC UNS DIN EN/DIN W-Nr.
NS 1404
BG2830
H 08028 N 08028
Sanicro 28
X1NiCrMoCu 31-27-4 1.4563
2 Approximate Comparison Table
United States International Organization for Standardization European Standard
UNS ISO Numerical Grade EN Numerical Grade
N08028 X1NiCrMoCu31-27-4 4563-080-28-I X1NiCrMoCu31-27-4 1.4563

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!