Grade X1NiMoCuN 25-20-7
European Standard Steel Grade 1.4529
Corresponding Standard EN 10250-4-1999
Open die steel forgings for general engineering purposes - Part 4: Stainless steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X1NiMoCuN 25-20-7 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 19 24 6 0.15
Maximum Value 0.02 0.5 1 0.03 0.01 21 26 7 0.25
X1NiMoCuN 25-20-7 Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤250* 650~850 ≥300 ≥35 ≥100
t≤250** 650~850 ≥300 ≥35 ≥60
1 Approximate Comparison Table Austenitic Stainless Steel
China United States International Organization for Standardization Germany European Standard
GB Commercial Grade UNS ISO Numerical Grade DIN EN/DIN W-Nr. EN Numerical Grade
25-6Mo Incoloy926 N08926 X1NiCrMoCuN25-20-7 4529-089-26-I X1NiCrMoCuN25-20-7 1.4529 X1NiCrMoCuN25-20-7 1.4529
2 Approximate Comparison Table Austenitic Stainless Steel
United States European Standard
ASTM EN Numerical Grade
N08926
NO8367
X1NiCrMoCuN25-20-7 1.4529