Grade X2CrNiMoN 25-7-4
European Standard Steel Grade 1.4410
Corresponding Standard EN 10250-4-1999
Open die steel forgings for general engineering purposes - Part 4: Stainless steels
Classification Duplex Stainless Steel
Properties Corrosion Resistance
X2CrNiMoN 25-7-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 24 6 3 0.2
Maximum Value 0.03 1 2 0.035 0.015 26 8 4.5 0.35
X2CrNiMoN 25-7-4 Mechanical Properties
diameter
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤160* 730~930 ≥530 ≥25 ≥100
t≤160** 730~930 ≥530 ≥20 ≥60
1 Approximate Comparison Table Austenitic-Ferritic Stainless Steel
China Japan United States International Organization for Standardization Germany European Standard
GB ISC JIS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. EN Numerical Grade
022Cr25Ni7Mo4N S25073 UR 47N+ 2507 S32750 X2CrNiMoN25-7-4 4410-327-50-E X2CrNiMoN25-7-4 1.4410 X2CrNiMoN25-7-4 1.4410
2 Approximate Comparison Table Austenitic-Ferritic Stainless Steel
United States France European Standard Sweden
UNS NF EN/NF EN Numerical Grade SS
S32750 Z3CND25-06Az X2CrNiMoN25-7-4 1.4410 2328

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!