Grade C45
European Standard Steel Grade 1.0503
Corresponding Standard EN 10277-2-2008
Bright steel products - Technical delivery conditions - Part 2: Steels for general engineering purposes
Classification Carbon Steel
C45 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo More
Minimum Value 0.42 - 0.5 - - - - - Cr+Mo+Ni≤0.63
Maximum Value 0.5 0.4 0.8 0.045 0.045 0.4 0.4 0.1
C45 Mechanical Properties
thickness
t
mm
Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
5≤t≤10 C45+C Cold Rolling (+C) 750~1050 ≥565 ≥5
10<t≤16 C45+C Cold Rolling (+C) 710~1030 ≥500 ≥6
16<t≤40 C45+C Cold Rolling (+C) 650~1000 ≥410 ≥7
40<t≤63 C45+C Cold Rolling (+C) 630~900 ≥360 ≥8
63<t≤100 C45+C Cold Rolling (+C) 580~850 ≥310 ≥8
16<t≤100 C45+SH Rolling and turning (+SH) 580~820 172~242
1 Approximate Comparison Table
China Japan International Organization for Standardization European Standard
GB JIS ISO EN Numerical Grade
45 S45C C45 C45 1.0503
2 Approximate Comparison Table
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
45 S45C 1042
1045
Gr.1043
C45 C45 AF65C45
C45
C45 1.0503 45 1650 070M46
50HS
3 Approximate Comparison Table
China Japan United States International Organization for Standardization France Russia United Kingdom
GB JIS ASTM/AISI ISO NF EN/NF GOST BS EN/BS
GB/T 699-1999
45
S45C 1045 ISO 630-1:1987
C45
C45E4
C45M2
C45
XC45
45 060A42
060A47

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!