Grade Z6CNNb18-12B
Corresponding Standard NF A 35-578-1991
Iron and Steel. Stainless Steel for High Temperature Application
Classification Austenitic Stainless Steel
Z6CNNb18-12B Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni B More
Minimum Value 0.04 - - - - 17 11 0.0015 Nb≥10×C
Maximum Value 0.08 0.75 2 0.04 0.015 19 13 0.006
Z6CNNb18-12B Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
+Q1050~1100 530~730 ≥215 ≥38